Corrosion of common metals according to ISO 9223

When the time of wetness (TOW) falls in category four (T4)

Chloride

Sulfur dioxide

Steel

Copper & Zinc

Aluminum

S0 or S1

P1

C3

C3

C3

..

P2

C4

C3-4

C3-4

..

P3

C5

C4-5

C4-5

S2

P1

C4

C4

C3-4

..

P2

C4

C4

C4

..

P3

C5

C5

C5

S3

P1

C5

C5

C5

..P2C5C5C5
..P3C5C5C5

Back to ISO 9223