MNL 20: Corrosion Tests and Standards - Application and Interpretation

Second Edition; Editor: Robert Baboian 

ASTM; Publication Date: 2004;   ISBN:0-8031-2098-2; Hard cover; 800 pages ($245) 

Revised and updated, the new edition of this highly respected publication provides guidelines for recognizing types of corrosion, as well as the fundamentals of testing. It provides the most recent technologies for making calculations, interpretations, and correlations, and serves as a source book for procedures, equipment, and standards used in testing. As and added bonus you get a complimentary CD of 115 ASTM and 60 NACE standards referenced throughout the book.

Eight sections cover:

General Information provides the tools to define, interpret, and evaluate the technology. Greatly expanded, this section includes a UNS for metals and alloys and their common names; standards terminology; SI and matrix guide; general conversion tables; corrosion rate calculations and all necessary conversion factors; and much more. :

Testing and Evaluation includes planning and design of tests, types of corrosion data, metallographic and surface analysis, statistical treatment of data, data computerization and computer applications:

Types of Tests examines laboratory-accelerated tests, field tests, and service tests. This section describes test techniques and specific considerations such as specimen preparation, test duration, acceleration factors, and pertinent standards:

Testing for Corrosion Types covers uniform, pitting, crevice, galvanic, intergranular, exfoliation, erosion, cavitation, fretting, dealloying, stress corrosion, corrosion fatigue and hydrogen damage:

Testing in Environment addresses outdoor and indoor atmospheres, seawater, fresh water, soils, concrete, industrial waters, industrial chemical, petroleum, high-temperature gases, organic liquids, molten salts, liquid metals, corrosion inhibitors, in-vivo, and microbiological effects. :

Materials Testing gives you an overview of important tests used in evaluating the corrosion behavior of metals and alloys, including zinc, lead, aluminum, steels, copper, nickel, stainless steels, cobalt-base alloys, titanium, zirconium and hafnium, tantalum and niobium alloys, metallic coatings on steel, nonmetallic coatings, metal matrix composites, electrodeposits, and powder metallurgy materials:

Testing in Industries provides an overview of corrosion testing unique to each industry, including automotive, commercial aircraft, military aircraft and equipment, pipeline, highways, tunnels and bridges, marine-piers and docks, electric power, nuclear power, steam generation, flue gas desulphurization, electronics, telecommunications, metal processing, chemical processing, pulp and paper, petroleum production and refining, food and beverage, water handling systems, medical and dental, and pharmaceutical:

Corrosion-Related Standards provides a comprehensive list of standards developed by various organizations including the American Petroleum Institute, American Waterworks Association, ASME International, ASTM International, International Electrotechnical Commission, ISO, NACE International, SAE International, and the Steel Structures Painting Council. :