Crevice Corrosion


Corrosion and cracking problems

... in a Boeing 737

Here, on the belly of a Boeing 737, the corrosion byproduct has expanded to the point where a number of rivets have actually popped their heads. Again, notice how the rivets appear to be sunken. (courtesy Mike Dahlager


 