Overpotential profile during  DC interference with current drainage

Figure 19 Overpotential along the pipeline for a train at position 2 in Figure 13 and with current drainage.


Study and Evaluation of Stray Current Influences on Cathodic Protection Systems of Buried Pipelines, L. Bortels, ELSYCA - Kranenberg 6 - 1731 - BELGIUM, ELSYCA