Resin Type |
Assign Value |
Active Pigment |
Assign Value |
Thickness /microns |
Assign Value |
|
Drying oil or Alkyd |
1 |
None |
1 |
<50 |
1 |
|
Epoxy, Polyurethane |
2 |
Micaceous Iron Oxide (MIO) |
2 |
50 -100 |
2 |
|
Aluminium Flake |
2 |
100 -200 |
3 |
||
|
Lamellar Glass Flake |
3 |
>200 |
4 |
||
|
Micronised glass flake |
2 |
This document was prepared on 10 November 2000 by Graham Gedge