Resin Type | Assign Value | Active Pigment | Assign Value | Thickness /microns | Assign Value |
Drying oil or Alkyd | 1 | Zinc Phosphate | 1 | <50 | 1 |
Epoxy, Polyurethane | 2 | Zinc rich (organic or silicate) | 3 | 50 -100 | 2 |
Red Lead | 4 | >100 | 3 | ||
Aluminium Flake | 2 |
This document was prepared on 10 November 2000 by Graham Gedge