Figure 5 Stray current density pattern along the foreign pipe for varying pipe-to-anode distances.
Study and Evaluation of Stray Current Influences on Cathodic Protection Systems of Buried Pipelines, L. Bortels, ELSYCA - Kranenberg 6 - 1731 - BELGIUM, ELSYCA