Predicting corrosion related electrical and magnetic fields using BEM

Robert Adey and John Baynham

Computational Mechanics BEASY Ltd

Ashurst Lodge, Ashurst, Southampton, Hampshire

This paper was edited for the Corrosion Doctors web site.