Changes occurring in seawater with depth at a Pacific ocean test site
The units have to be estimated with the following conversion:
Temperature: scale x 1 (oC)
Oxygen: scale x 0.333 (ppm)
pH: 6.4 + scale x 0.1 (pH unit)
Salinity: 33.0 + scale x 0.1 (o/oo)