Total Dissolved Solids

If TDS is unknown, but conductivity is, one can estimate mg/L TDS using a conversion table such as the one presented here.

Conductivity

TDS 

 ( micro-mho/cm)

(mg/L as CaCO3)

1

0.42

10.6

4.2

21.2

8.5

42.4

17.0

63.7

25.5

84.8

34.0

106.0

42.5

127.3

51.0

148.5

59.5

169.6

68.0

190.8

76.5

212.0

85.0

410.0

170.0

610.0

255.0

812.0

340.0

1008.0

425.0